I've had my new 642 about 2 months. Much carry and ~200 rounds. Always carried alone in a pocket holsterwith no keys, etc. to contact finish.
Despite my care, there appears to be the beginning of surface flaking on 1 or 2 high spots.
Is this characteristic of the materials of construction/finish.. live with it or a manufacturing defect ?
Thanks
Despite my care, there appears to be the beginning of surface flaking on 1 or 2 high spots.
Is this characteristic of the materials of construction/finish.. live with it or a manufacturing defect ?