Hot blues are labor intensive and a bit hazardous, but not that expensive. I made a pan from mild steel and got the lye and nitrates from a drug store. Stovetop heat source. Still have the scars from that lye!
These days, Brownells and others sell bluing salts, tanks, and all the polishing gear.