Everybody who sent me a PM, my box was full and I did not receive any.
The BHN 12 .38 bullets were cast out of a 1.3% tin, 4% antimony alloy I made with lead and linotype, the BHN 16 bullets - .40 and the 160gr .38 were cast with foundry hardball lead (2% tin, 6% antimony) from Mayco industries. I tried the casting business and it did not work out, so I closed it and am selling off what's left. I have about 50 000 of the 158gr .38, about 25 000 of the 125 gr .38, about 15 000 of the 160 gr .38 and probably 5-6000 of the .40 cal's left.
I am in Windermere, just north of Disney's Magic Kingdom.

Edit: It takes too long to figure the 3% credit card fee, so I'm not going to bother with it. I can also mix the bullets in smaller increments if you prefer to try them this way - for example I can send you 250 125gr. 38 and 250 158gr .38 instead of 500 of the same bullets.

Last edited by gotin; 12-08-2012 at 05:28 PM.