$19 each is a pretty good deal.
But, they don't drop as fast out of the shoot as does factory/coated mags. So, I took the 6 I ordered and cleaned/degreased them and then coated the with AluminHyde II (flat black).
I used my heat gun for 2-3 min on each one to do a quick dry off and they will sit for 2 weeks to cure.
A quick test with one and it now ejects just as nicely as the original equipment ones.
I plan to lube the springs and the inside with Miltec-1 and heat to 200F before reassembling.
Parkerizing is good, Miltec-1 properly applied is better.
But, they don't drop as fast out of the shoot as does factory/coated mags. So, I took the 6 I ordered and cleaned/degreased them and then coated the with AluminHyde II (flat black).
I used my heat gun for 2-3 min on each one to do a quick dry off and they will sit for 2 weeks to cure.
A quick test with one and it now ejects just as nicely as the original equipment ones.
I plan to lube the springs and the inside with Miltec-1 and heat to 200F before reassembling.
Parkerizing is good, Miltec-1 properly applied is better.